Influence of High Current-Density Impulses on the Stress-Strain Response and Microstructural Evolution of the Single Crystal Superalloy CMSX-4

Influence of High Current-Density Impulses on the Stress-Strain Response and Microstructural Evolution of the Single Crystal Superalloy CMSX-4

Categories Journals
Year 2018
Authors Demler, E.; Gerstein, G.; Dalinger, A.; Epishin, A.; Heidenblut, T.; Nürnberger, F.; Maier, H. J.
Published in Materials Research 21, 2018 (6), 1063
DOI 10.1590/1980-5373-MR-2018-0428